Inconel 625 and 718

Machining Superalloy Inconel 625 and Inconel 718

Superalloys Inconel 625 and Inconel 718

The superalloys Inconel 625 and Inconel 718 are used in the motorsport applications.

In this case the H.I.P. (Hot Isostatic Pressing) is carried out as post-melting treatment while the CNC machining and the 3D testing are carried out only if necessary.

The superalloy Inconel 625 can be processed with:

  • Investment Casting and CNC machining

Superalloys Inconel 625 and Inconel 718 key strengths

  • High quality surface
  • Excellent thickness control
  • Resistance to high temperatures